Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0129 cm/cm | 0.0129 in/in | ASTM D955 |
Multibase Multi-Flex® TPE D 4310 Multi-Flex® D 4310 Natural was designed to replace Himont's CA 53 G material. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.0129 cm/cm | 0.0129 in/in | |
Plastcom SLOVAMID 66 MI PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |