Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0109 cm/cm | 0.0109 in/in | ASTM D955 |
RheTech Products HP505-01 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Glove box binConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0109 cm/cm | 0.0109 in/in | ASTM D955 |
Plenco 7500 Phenolic, Granular, Injection Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Linear Mold Shrinkage | 0.0109 cm/cm | 0.0109 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0339T20L1 Talc Reinforced |