Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | ISO 2577 |
Panjin Zhongrun Chemerize 012P High Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF1030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | Injection and Compression; ISO 2577 |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ISO 2577 |
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.015 cm/cm | 0.0070 - 0.015 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 TF-GV 1520 Nylon 6 for injection molding, 15% PTFE lubricated, 20% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® NJ-10GF/000 Nylon 12 - 10% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | ASTM D955 |
Kolon SPESIN® KP213G15SIBL Glass Fiber Reinforced PBT Compound Resin G/F 15%, high toughness, excellent surfaceApplications: Various types of housingsInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D1299 |
Loxim 820 12 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | ASTM D955 |
Kolon KOPA® KN133G20 G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm @Thickness 3.18 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
LyondellBasell Hifaxâ„¢ HSBMR246 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ HSBMR246 medium high melt flow, 1,500 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an outstanding balance of physical pro.. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
Techmer ES Plaslube® PC-50/TF/15 NAT Polycarbonate |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
Techmer ES Plaslube® PC-50/TF/22 NAT Polycarbonate |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
PlastxWorld CEVIAN® B1500 PBT/ABS Alloy Unfilled, Excellent ToughnessThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Linear Mold Shrinkage | 0.0070 - 0.011 cm/cm @Thickness 3.20 mm |
0.0070 - 0.011 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0080 cm/cm @Thickness 1.59 mm |
0.0070 - 0.0080 in/in @Thickness 0.0625 in |
plaque |
Lubrizol Estane® 2103-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | |
Ecomass® 1850ZC84 Stainless Steel Powder Filled Polyamide (PA6), Injection Molding Stainless Steel Powder Filled Polyamide (PA6), Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shielding a.. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | |
E-Polymers TEKAMID® H14HR High Toughness Heat Resistance PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Copolymer CP0436W30L Wollastonite Reinforced |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0336M30CL Mica Reinforced Coupled |
|||
Linear Mold Shrinkage | 0.0070 - 0.0083 cm/cm | 0.0070 - 0.0083 in/in | IS 13411-1992 |
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
A. Schulman ComAlloy Hiloy® 164 Polypropylene, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
Asahi Kasei Thermylene® P1-10FG-8100 10% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
Ashley Polymers Ashlene® 520-13G Nylon 66, 13% Glass Reinforced 13% Glass reinforced Nylon 66.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | |
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | ISO 2577 |
Panjin Zhongrun Chemerize 021P Medium Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | |
E-Polymers TEKAFIN® PH50GM 30% Glass Fiber Reinforced Mineral Filled Low Warpage Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |