Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0059 cm/cm | 0.0059 in/in | Bayer Test |
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, 20% Mineral Filled, MDI-based 2-Component Liquid System 0.1 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offi.. |
|||
Linear Mold Shrinkage | 0.0059 cm/cm | 0.0059 in/in | |
Cytec EN-2523 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |