Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
RheTech Products FT7012-707UV Thermoplastic Polyolefin, UV Stabilized, 848 Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | STN 64 0808 |
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Plastcom SLOVASTER® B GF 50 PBT, 50% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 50% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Oxford Polymers 10GF 10% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding 10% Glass Fiber Filled Polyetherimide for Extrusion and Injection MoldingInformation provided by Oxford Polymers. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM Data; MD |
Styrolution Terluran® HH-106 ABS Terluran HH-106 is an injection molding ABS grade with high resistance to heat deformation and impact.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM Data; MD |
Styrolution Terlux® 2802 TR MABS Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 2645 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 275 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 345 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 9030 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 941 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnumâ„¢ PG914 ABS, High Impact MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 358HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Polyram PlusTek PB302G3 Nylon 6, 15% Glass Fiber 15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Dow AIM® 4800 High Impact Styrenic Resin AIM® 4800 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell BJ-34 Nylon 6, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell BR-13 Nylon 6, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell AJ-34 Nylon 66, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell BR-33 Nylon 6, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell BT-34 Nylon 6, 20% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM Data; MD |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Conditioned) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | restricted |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | restricted |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
BASF Ultramid® B3S HP PA6 (Conditioned) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | LATI |
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |