Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0033 cm/cm
0.0033 in/in
per ATM D955. Post shrinkage is 0.13% at 72hr 120ºC per ASTM D1299.
Plenco 4100 Phenolic, Granular, Compression Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and ..
Linear Mold Shrinkage 0.0033 cm/cm
0.0033 in/in
ASTM D955
Plenco 08235 Polyester BMC, Compression Molded
PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable ..
Linear Mold Shrinkage 0.0033 cm/cm
0.0033 in/in
ASTM D955
Plenco 6343 Phenolic, Granular, Transfer Molded
PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz..
Linear Mold Shrinkage 0.0033 cm/cm
0.0033 in/in
ASTM D955
Plenco 4311 Phenolic, Granular, Compression Molded
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized..
Linear Mold Shrinkage 0.0033 cm/cm
0.0033 in/in
restricted
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Conditioned)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Linear Mold Shrinkage 0.0033 cm/cm
0.0033 in/in
restricted
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..