Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00310 cm/cm | 0.00310 in/in | cure shrinkage |
Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy Ceramic-Filled, Low Expansion, High Lap-Shear Strength & Chemical Resistance, Low Outgassing. |