Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | |
NatureWorks® Ingeo™ 3001D Injection Grade PLA NatureWorks® PLA (polylactide) polymer 3001D is designed for injection molding applications. It is designed for clear applications with heat deflection temperatures lower than 130ºF (55ºC). Appli.. |
|||
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | |
NatureWorks® Ingeo™ 3052D Lubricated, High Flow Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. It is designed for injection molding applications where the requirements are clarity with heat def.. |
|||
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | |
NatureWorks® Ingeo™ 3251D Injection Grade PLA IngeoTM Biopolymer 3251D is designed for injection molding applications. This polymer grade has a higher melt flow capability than other IngeoTM resins currently in the market place. The higher flow.. |
|||
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | |
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip.. |
|||
Linear Mold Shrinkage | 0.003 - 0.006 cm/cm | 0.003 - 0.006 in/in | |
NatureWorks® Ingeo™ AW 300D Injection Grade Biopolymer Specifically designed for use in injection molded food serviceware applications. This opaque, off-white molding grade creates parts that are rigid and heat resistant for tableware used with hot food.. |