Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0021 cm/cm | 0.0021 in/in | ASTM D955 |
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0021 cm/cm | 0.0021 in/in | ATM D955 |
Plenco 50015 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu.. |
|||
Linear Mold Shrinkage | 0.0021 cm/cm | 0.0021 in/in | ASTM D955 |
Plenco 7556 Phenolic, Briquette, Injection Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |