Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000600 - 0.0130 cm/cm | 0.000600 - 0.0130 in/in | Average value: 0.00759 cm/cm Grade Count:23 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.000600 - 0.00350 cm/cm | 0.000600 - 0.00350 in/in | Average value: 0.00197 cm/cm Grade Count:23 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.000600 - 0.0135 cm/cm | 0.000600 - 0.0135 in/in | Average value: 0.00401 cm/cm Grade Count:82 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.000600 - 0.0160 cm/cm | 0.000600 - 0.0160 in/in | Average value: 0.00542 cm/cm Grade Count:110 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage | 0.000600 - 0.0300 cm/cm | 0.000600 - 0.0300 in/in | Average value: 0.00621 cm/cm Grade Count:175 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Linear Mold Shrinkage | 0.000600 - 0.00250 cm/cm | 0.000600 - 0.00250 in/in | Average value: 0.00138 cm/cm Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is.. |
|||
Linear Mold Shrinkage | 0.000600 - 0.0200 cm/cm | 0.000600 - 0.0200 in/in | Average value: 0.00418 cm/cm Grade Count:208 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |