Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000 - 0.0200 cm/cm | 0.000 - 0.0200 in/in | Average value: 0.00468 cm/cm Grade Count:268 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0250 cm/cm | 0.000 - 0.0250 in/in | Average value: 0.00452 cm/cm Grade Count:531 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00600 cm/cm | 0.000 - 0.00600 in/in | Average value: 0.00223 cm/cm Grade Count:50 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.000 - 0.0160 cm/cm | 0.000 - 0.0160 in/in | Average value: 0.00232 cm/cm Grade Count:146 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00900 cm/cm | 0.000 - 0.00900 in/in | Average value: 0.00184 cm/cm Grade Count:17 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.000 - 0.0300 cm/cm | 0.000 - 0.0300 in/in | Average value: 0.00259 cm/cm Grade Count:88 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0100 cm/cm | 0.000 - 0.0100 in/in | Average value: 0.00164 cm/cm Grade Count:50 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0150 cm/cm | 0.000 - 0.0150 in/in | Average value: 0.00533 cm/cm Grade Count:3 |
Overview of materials for PVC, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00500 cm/cm | 0.000 - 0.00500 in/in | Average value: 0.00133 cm/cm Grade Count:40 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00400 cm/cm | 0.000 - 0.00400 in/in | Average value: 0.00126 cm/cm Grade Count:39 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00200 cm/cm | 0.000 - 0.00200 in/in | Average value: 0.000869 cm/cm Grade Count:12 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00300 cm/cm | 0.000 - 0.00300 in/in | Average value: 0.00100 cm/cm Grade Count:19 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.000 cm/cm | 0.000 in/in | Average value: 0.000 cm/cm Grade Count:4 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0100 cm/cm | 0.000 - 0.0100 in/in | Average value: 0.00531 cm/cm Grade Count:104 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00200 cm/cm | 0.000 - 0.00200 in/in | Average value: 0.000760 cm/cm Grade Count:5 |
Overview of materials for Phenolic, Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.000 - 0.00600 cm/cm | 0.000 - 0.00600 in/in | Average value: 0.00210 cm/cm Grade Count:18 |
Overview of materials for Polyphenylene Sulfide (PPS), Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.000 - 0.0220 cm/cm | 0.000 - 0.0220 in/in | Average value: 0.00607 cm/cm Grade Count:207 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Linear Mold Shrinkage | 0.000 - 0.0120 cm/cm | 0.000 - 0.0120 in/in | Average value: 0.00205 cm/cm Grade Count:38 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00100 cm/cm | 0.000 - 0.00100 in/in | Average value: 0.000449 cm/cm Grade Count:12 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0160 cm/cm | 0.000 - 0.0160 in/in | Average value: 0.00477 cm/cm Grade Count:49 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0230 cm/cm | 0.000 - 0.0230 in/in | Average value: 0.00449 cm/cm Grade Count:704 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0100 cm/cm | 0.000 - 0.0100 in/in | Average value: 0.00385 cm/cm Grade Count:79 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0400 cm/cm | 0.000 - 0.0400 in/in | Average value: 0.00583 cm/cm Grade Count:27 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |