Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | >= 15000 hour @Temperature 50.0 °C |
>= 15000 hour @Temperature 122 °F |
No Failure after 15,000 hours; Igepal CO630; ASTM D1693 |
LyondellBasell Montell 0300 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenesApplications: packaging industry, minor additive.. |
|||
ESCR 10% Igepal® | >= 15000 hour @Temperature 50.0 °C |
>= 15000 hour @Temperature 122 °F |
No Failure after 15,000 hours; Igepal CO630; ASTM D1693 |
LyondellBasell Montell 0800 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptableApplications: concrete carrierMe.. |
|||
ESCR 10% Igepal® | >= 15000 hour @Temperature 50.0 °C |
>= 15000 hour @Temperature 122 °F |
No Failure after 15,000 hours; Igepal CO630; ASTM D1693 |
LyondellBasell DP 0110M Polybutene Key Features: highly isotactic, semi-crystalline nucleated homopolymer, good creep resistance, good environmental stress crack resistance, FDA acceptable, easily dispersibleApplications: packaging i.. |