Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 2000 dtex | 1800 denier | |
COI Ceramics Nicalon™ CG SiCO Ceramic Fiber Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties .. |
|||
Fiber Count | 2000 dtex | 1800 denier | |
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber Description: Manufactured near-oxygen-free using electron-beam curing. The fiber is homogeneously composed of ultrafine beta-SiC crystallites and carbon. The fiber has excellent strength and modulus.. |
|||
Fiber Count | 2000 dtex | 1800 denier | |
COI Ceramics Nicalon™ HRV SiCO Ceramic Fiber Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties .. |
|||
Fiber Count | 2000 dtex | 1800 denier | roving |
3M Nextel™ AF-20 Industrial Woven Fabric 312 Information provided by 3M |
|||
Fiber Count | 2000 dtex | 1800 denier | 1/2 |
3M Nextel™ AF-30 Industrial Woven Fabric 312 Information provided by 3M |
|||
Fiber Count | 2000 dtex | 1800 denier | 1/2 |
3M Nextel™ AF-40 Industrial Woven Fabric 312 Information provided by 3M |
|||
Fiber Count | 2000 dtex | 1800 denier | 1/2 |
3M Nextel™ AF-62 Industrial Woven Fabric 312 Information provided by 3M |