Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 11.0 - 22.0 dtex | 9.90 - 19.8 denier | |
EMS-Griltech Grilon® CM 2600 White Nylon 6 Fiber Description: GRILON CM 2600 is a Nylon 6 technical fiber which is used to produce technical felts.Data provided by EMS-Griltech. |
|||
Fiber Count | 17.0 - 22.0 dtex | 15.3 - 19.8 denier | |
EMS-Griltech Grilon® TN 2200 White Nylon 6 Fiber Description: GRILON TN 2200 is used for woolen yarns which is then further processed to produce technical fabrics.Applications: Press Felt FabricData provided by EMS-Griltech. |