Polymer Property : Fiber Count = 422 dtex Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Fiber Count 422 dtex
380 denier
Warp yarn; Kevlar® 49
Hexcel® HexForce™ 348 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
Fiber Count 422 dtex
380 denier
Fill yarn; Kevlar® 49
Hexcel® HexForce™ 348 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
Fiber Count 422 dtex
380 denier
Warp yarn; Kevlar® 49
Hexcel® HexForce™ 351 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
Fiber Count 422 dtex
380 denier
Fill yarn; Kevlar® 49
Hexcel® HexForce™ 351 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..