Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Melt Index | 50 g/10 min | 50 g/10 min | I<sub>2</sub>; ASTM D1238 |
Lotte Chemical Titan TITANEX® LI5011 Linear low density polyethylene resin
(discontinued **) LI5011 is a pelleted high flow linear low density polyethylene. The higher melting point of the resin allows for higher end-use temperatures.Applications: House-wares, toys, lids, containers.Advan.. |
|||
Base Resin Melt Index | 50 g/10 min @Temperature 230 °C |
50 g/10 min @Temperature 446 °F |
ASTM D1238 |
Lotte Chemical Titan TITANPRO® PM803 Polypropylene homopolymer Titanpro® PM803 is a high flow and also a controlled rheology grade. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (.. |