Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin
(discontinued **) LF1043 is a pelleted linear low density polyethylene resin formulated with antioxidant, and antiblock agent. This product is used for blown film extrusion which offers outstanding toughness, extrud.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LF1044 Linear low density polyethylene resin
(discontinued **) LF1044 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and draw down.. |
|||
Base Resin Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LF2024 Linear low density polyethylene resin
(discontinued **) LF2024 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and .. |
|||
Base Resin Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin
(discontinued **) LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and .. |
|||
Base Resin Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LF0754 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF0754 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant agent. This product is used for blown film extrusion which offers outstanding toughness, extrudabilit.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LF1054 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF1054 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and .. |
|||
Base Resin Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LF2554 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF2554 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for slot cast extrusion which offers outstanding toughness, extrudability and d.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin
(discontinued **) LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.Applications: House-wares, lids, closures and toys.Advantages: Excellent stress crack resistance,.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin
(discontinued **) Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL216 Linear low density polyethylene resin
(discontinued **) Titanceed® mL216 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL2764 Linear low density polyethylene resin
(discontinued **) Titanceed® mL2764 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL2764 have outstanding tensile properties, impact streng.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL3564 Linear low density polyethylene resin
(discontinued **) Titanceed® mL3564 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL3564 have outstanding tensile properties, impact streng.. |
|||
Base Resin Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services
(discontinued * VORIDIAN HIFOR CLEAR SC74558-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives. Films produced with t.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D4883 |
Eastman 1550F Film Polyethylene
(discontinued **) Polyethylene 1550F is a low density polyethylene that contains no additives.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no long.. |
|||
Base Resin Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D4883 |
Eastman E6838-902F Polyethylene Film
(discontinued **) Polyethylene E6838-902F natural contains slip and antiblock and is suggested for film applicationsApplications/UsesFood - contact applicationsEastman Chemical Company sold its polyethylene business .. |
|||
Base Resin Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANLENE® LDI300YY Low density polyethylene resin LDI300YY is a low density polyethylene resin for injection molding and is a barefoot grade. LDI300YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2.. |
|||
Base Resin Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANLENE® LDC800YY Low density polyethylene resin LDC800YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC800YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2.. |
|||
Base Resin Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANLENE® LDC801YY Low density polyethylene resin LDC801YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC801YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2.. |