Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2242 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |