Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® MR4086 Medium density polyethylene resin
(discontinued **) MR4086 is a UV stabilized, pelleted medium density polyethylene for rotomolding.Applications: Large industrial tanks, agriculture tanks, chemical drums, bins, cones, bottle caps.Advantages: Excelle.. |