Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LI5011 Linear low density polyethylene resin
(discontinued **) LI5011 is a pelleted high flow linear low density polyethylene. The higher melting point of the resin allows for higher end-use temperatures.Applications: House-wares, toys, lids, containers.Advan.. |