Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 1700 ppm | 1700 ppm | |
ExxonMobil LL 1002x74 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Slip Level | 1700 ppm | 1700 ppm | |
ExxonMobil LL 1002x79 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Slip Level | 1700 ppm | 1700 ppm | |
ExxonMobil LL 1001x74 Blown Film Resin LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Slip Level | 1700 ppm | 1700 ppm | |
ExxonMobil LL 1107x95 Blown Film Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Slip Level | 1700 ppm | 1700 ppm | |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Slip Level | 1700 ppm | 1700 ppm | |
ExxonMobil LLDPE LL 1107X95 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |