Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 900000 - 1.50e+6 g/mol | 900000 - 1.50e+6 g/mol | |
Lucite International Colacryl ® D120 Acrylic Dental Resin A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f.. |
|||
Molecular Weight | 900000 - 1.50e+6 g/mol | 900000 - 1.50e+6 g/mol | |
Lucite International Colacryl ® D150 Acrylic Dental Resin A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f.. |
|||
Molecular Weight | 900000 - 1.50e+6 g/mol | 900000 - 1.50e+6 g/mol | |
Lucite International Colacryl ® D60 Acrylic Dental Resin A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f.. |
|||
Molecular Weight | 900000 - 1.50e+6 g/mol | 900000 - 1.50e+6 g/mol | |
Lucite International Colacryl ® D80 Acrylic Dental Resin A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f.. |
|||
Molecular Weight | 900000 - 1.50e+6 g/mol | 900000 - 1.50e+6 g/mol | |
Lucite International Colacryl ® PD12 Acrylic Dental Resin Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties... |
|||
Molecular Weight | 900000 - 1.50e+6 g/mol | 900000 - 1.50e+6 g/mol | |
Lucite International Colacryl ® PD2 Acrylic Dental Resin A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f.. |
|||
Molecular Weight | 900000 - 1.50e+6 g/mol | 900000 - 1.50e+6 g/mol | |
Lucite International Colacryl ® TS 1649 Acrylic Orthodontic Polymer A range of methacrylate based copolymers designed for the manufacture of high quality orthodontic dental resins.Features: Excellent dry flow characteristics; Closely controlled particle size; Contai.. |
|||
Molecular Weight | 900000 - 1.50e+6 g/mol | 900000 - 1.50e+6 g/mol | |
Lucite International Colacryl ® TS 1672 Acrylic Orthodontic Polymer A range of methacrylate based copolymers designed for the manufacture of high quality orthodontic dental resins.Features: Excellent dry flow characteristics; Closely controlled particle size; Contai.. |
|||
Molecular Weight | 900000 - 1.50e+6 g/mol | 900000 - 1.50e+6 g/mol | |
Lucite International Colacryl ® TS1785 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I.. |
|||
Molecular Weight | 900000 - 1.50e+6 g/mol | 900000 - 1.50e+6 g/mol | |
Lucite International Colacryl ® PD11SG Acrylic Dental Resin Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties... |