Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 43000 g/mol | 43000 g/mol | Weight average M |
Pearl Engineering PEPLPET B-101C PET Sheet Grade A sheet grade polymer used in thick films. |
|||
Molecular Weight | 43000 g/mol | 43000 g/mol | Weight average M |
Pearl Engineering PEPLPET B-103C PET Bottle Grade A co-polymer used for mineral water bottles |