Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 374.5 g/mol | 374.5 g/mol | |
Dow Corning Z-6032 SILANE DOW CORNING Z6032 contains a vinylbenzyl and amine organic and a trimethoxysilyl inorganic group. The product is supplied in methanol. Possessing both organic and inorganic reactivity, DOW CORNING Z.. |