Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 25000 g/mol | 25000 g/mol | |
Unitika elitel UE3220 Polyester, Flake Adhesive agent, Resin modifier, Soft type, Standard resinUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as a.. |
|||
Molecular Weight | 25000 g/mol | 25000 g/mol | |
Unitika elitel UE3400 Polyester, Flake Elastomer, Rubber elasticity, Wide compatibility, Low temperature flexibilityUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications fro.. |