Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 120000 g/mol | 120000 g/mol | |
Ineos ABS Lustran® SMA 245 SMA Copolymer Lustran® SMA 245 is a Styrene Maleic Anhydride copolymer manufactured at a target maleic anhydride level of 25%. The process used for making Lustran® SMA 245 yields a product with good clarity.. |