Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 12000 g/mol | 12000 g/mol | |
Lucite International Elvacite ® 4044 Acrylic Resin Elvacite® 4044 is a solid bead resin is a medium molecular weight butyl methacrylate-methyl methacrylate copolymer. It is a relatively soft and flexible acrylic resin for use in manufacture of ce.. |
|||
Molecular Weight | 12000 g/mol | 12000 g/mol | |
Westlake Epolene® E-25 Chemically Modified Polypropylene, Maleation Processed Product Description: Epolene E-25 is a maleic anhydride grafted polypropylene recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emul.. |
|||
Molecular Weight | 12000 g/mol | 12000 g/mol | |
Westlake Epolene® N-15 Nonemulsifiable - Low Molecular Weight Polypropylene Polymer Product Description: Epolene N-15 is a low viscosity polypropylene homopolymer with a high melt point and excellent hardness. Epolene N-15 is used in color concentrates, toner compounds, and as a pi.. |
|||
Molecular Weight | 12000 g/mol | 12000 g/mol | |
Westlake Epolene® N-15P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-15P is a low viscosity polypropylene homopolymer powder with a high melt point and excellent hardness. Epolene N-15P is used in color concentrates, toner compounds, and as a p.. |