Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 101.96 g/mol | 101.96 g/mol | |
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam.. |
|||
Molecular Weight | 101.96 g/mol | 101.96 g/mol | |
American Elements A-MITE™ Aluminum Oxide Nanopowder General DescriptionApplicationsA-MITE™ powders and dispersions are recently developed inorganic aluminium oxide nanoparticles with unique abrasion resistance properties for use in optical lenses, w.. |
|||
Molecular Weight | 101.96 g/mol | 101.96 g/mol | |
Mateck Sapphire (Al2O3) Optical crystals |