Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 100000 g/mol | 100000 g/mol | ASTM D3536 |
SK Chemicals SKYTHANE® U0251M Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Molecular Weight | 100000 g/mol | 100000 g/mol | ASTM D3536 |
SK Chemicals SKYTHANE® UB601 Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Molecular Weight | 100000 g/mol | 100000 g/mol | |
Westlake Epolene® C-17 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer Product Description: Epolene C-17 is a branched low density polyethylene with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wa.. |
|||
Molecular Weight | 100000 g/mol | 100000 g/mol | |
Westlake Epolene® C-17P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer Description: Epolene C-17P is a branched low density polyethylene powder with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wa.. |