Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 7500 g/mol | 7500 g/mol | |
Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: Epolene E-20 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness and low color. It has a low softening point and low viscosity, which give .. |
|||
Molecular Weight | 7500 g/mol | 7500 g/mol | |
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: EE-2 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness. It is an excellent asphalt modifier which mixes readily with all asphalts. It h.. |