Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 670 g/mol | 670 g/mol | Mw; ETM 300-83 |
ExxonMobil ESCOREZ™ 5300 Petroleum Hydrocarbon Resin The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, APP an d A.. |
|||
Molecular Weight | 670 g/mol | 670 g/mol | Mw; ETM 300-83 |
ExxonMobil ESCOREZ™ 5400 Petroleum Hydrocarbon Resin Light colored cycloaliphatic hydrocarbon resin. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, natural rubber, synthetic polyisoprene, poly.. |
|||
Molecular Weight | 670 g/mol | 670 g/mol | |
3M Fluorinert™ FC-43 Electronic Liquid 3M™ Fluorinert™ Liquid FC-43 is a non-conductive, thermally and chemically stable liquid ideal for many single phase heat transfer fluid applications, especially in the electronics and semiconduct.. |