Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 58.1 g/mol | 58.1 g/mol | |
MV Labs K500 KF Potassium fluoride Information provided by MV Laboratories. |
|||
Molecular Weight | 58.1 g/mol | 58.1 g/mol | |
BASF Propionaldehyde Formula: C3H6OCAS: 123-38-6Description: Propionaldehyde is a colorless liquid, with a pungent odor. It is miscible in water in all proportions and is soluble in other organic solvents.Synonyms: Prop.. |