Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 547 g/mol | 547 g/mol | Theoretical |
PolyOne Synplast™ NOTM-E Tri (n-octyl) Trimellitate Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Molecular Weight | 547 g/mol | 547 g/mol | Theoretical |
PolyOne Synplast™ NOTM-PPC Tri (n-octyl) Trimellitate CPSIA HR 4040 Compliant Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Molecular Weight | 547 g/mol | 547 g/mol | Theoretical |
PolyOne Synplast™ TOTM-E Tri (2-ethylhexyl) Trimellitate Branched C8 trimellitate ester with antioxidantContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Molecular Weight | 547 g/mol | 547 g/mol | Theoretical |
PolyOne Synplast™ TOTM-N Tri (2-ethylhexyl) Trimellitate Branched C8 trimellitate esterInformation provided by PolyOne |
|||
Molecular Weight | 547 g/mol | 547 g/mol | |
LG Chemical TOTM Plasticizer Features: LG TOTM is used in cable and sheet by product that aging property and migration resistance among our products are superior.Application: Power cableInformation provided by LG Chemical |