Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 517.81 g/mol | 517.81 g/mol | |
Indium Corp. In2(SO4)3 Indium Sulfate Anhydrous Indium Sulfate is a grayish-white powder. It is hydroscopic and possesses a monoclinic prism structure. It is available as an anhydrous powder, a hydrated salt with 9 moles of associated water, an.. |