Polymer Property : Molecular Weight = 21500 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 21500 g/mol
21500 g/mol
Number average M
Pearl Engineering PEPLPET B-103C PET Bottle Grade