Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 2100 - 3000 g/mol | 2100 - 3000 g/mol | |
Suqian Unitechem Light Stabilizer 944 Chemical Name: Poly-{[6-[(1,1,3,3-tetramethylbutyl)amino]-1,3,5-triazine-2,4-diyl][(2,2,6,6-tetramethyl-4-piperidyl)imino]-1,6-hexanediyl[(2,2,6,6-tetramethyl-4-piperidyl)imino]}CAS NO.: 70624-18-9M.. |
|||
Molecular Weight | 2100 g/mol | 2100 g/mol | Mw; ETM 300-83 |
ExxonMobil ESCOREZ™ 1304 Petroleum Hydrocarbon Resin Premium aliphatic hydrocarbon resin which is designed to tackify a variety of adhesive polymers including EVA, metallocene polyolefines, APP, APAO, natural rubber, synthetic polyisoprene, polyisobut.. |