Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 113.16 g/mol | 113.16 g/mol | |
BASF Caprolactam Liquid Recommended use: Initial product for chemical syntheses, for the production of homopolymerisates and copolymerisatesInformation provided by BASF |
|||
Molecular Weight | 113.16 g/mol | 113.16 g/mol | |
BASF Caprolactam Tablets Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical synthesesInformation provided by BASF |