Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Aluminum Nanoparticles General DescriptionAluminum (Al) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Aluminum Particles are typically 10-30 nanometers (nm) with sp.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Antimony Nanoparticles General DescriptionAntimony (Sb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Antimony Particles are typically 20-40 nano.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Antimony Tin Oxide Nanoparticles General DescriptionAntimony Tin Oxide (ATO) Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. N.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Barium Titanate nanoparticles General DescriptionBarium Titanate Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nanoscale .. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Calcium Carbonate Nanoparticles General DescriptionCalcium Carbonate (CaCO3) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Carbonate Particles are typically 10 - 80 nanometers (.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Dysprosium Nanoparticles General DescriptionDysprosium (Dy) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 10 - 80 nanometers (nm) with sp.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Gadolinium Nanoparticles General DescriptionGadolinium (Gd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Gadolinium Particles are typically 10 - 45 nanometers (nm) with sp.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Indium Nanoparticles General DescriptionIndium (In) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Indium Particles are typically 20-40 nanomete.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Iron Cobalt Nanopowder General DescriptionIron Cobalt ( FeCo) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Iron Nanoparticles General DescriptionIron (Fe) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Iron Particles are typically 20-40 nanometers (.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Iron Nickel Nanopowder General DescriptionIron Nickel ( FeNi) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nano.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Iron Oxide Nanopowder General DescriptionIron Oxide ( Fe2O3 and Fe3O4) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure part.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Lanthanum Nanoparticles General DescriptionLanthanum (La) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lanthanum Particles are typically 5 - 40 nanometers (nm) with speci.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Lead Oxide Nanopowder General DescriptionLead Oxide ( PbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Lead Oxide Par.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Lithium Nanoparticles General DescriptionLithium (Li) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lithium Particles are typically 10 - 50 nanometers (nm) with specific.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Manganese Nanoparticles General DescriptionManganese (Mn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Manganese Particles are typically 20-40 na.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Nickel Nanoparticles General DescriptionNickel (Ni) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Nickel Particles are typically 10 - 40 nanometers (nm) with specific s.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Nickel Titanium Nanoparticles General DescriptionNickel Titanium (NiTi) Nanoparticles, nanodots or nanopowder are black spherical high surface area alloy particles. Nanoscale Nickel Titanium Particles are typically 10 - 40 nanom.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Niobium Nanoparticles General DescriptionNiobium (Nb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Niobium Particles are typically 10-20 nanometers (nm) with.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Praseodymium Nanoparticles General DescriptionPraseodymium (Pr) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Praseodymium Particles are typically 10 - 45 nanometers (nm) wit.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Samarium Nanoparticles General DescriptionSamarium (Sm) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Samarium Particles are typically 10 - 50 nanometers (nm) with specif.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Strontium Carbonate Nanoparticles General DescriptionStrontium Carbonate (SrCO3) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Strontium Carbonate Particles are typically 5 - 40 nan.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Terbium Nanoparticles General DescriptionTerbium (Tb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Terbium Particles are typically 10 - 80 nanometers (nm) with specific.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Tin Nanoparticles General DescriptionTin (Sn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tin Particles are typically 10-20 nanometers (nm) with specifi.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Ytterbium Nanoparticles General DescriptionYtterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with spec.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Yttrium Nanoparticles General DescriptionYttrium (Y) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Yttrium Particles are typically 5 - 45 nanometers (nm) with specific s.. |
|||
Specific Surface Area | 30 - 80 m²/g | 30 - 80 m²/g | |
American Elements Zirconium Nanoparticles General DescriptionZirconium (Zr) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Zirconium Particles are typically 10-40 nanometers (nm) with .. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Cerium Nanoparticles General DescriptionCerium (Ce) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Cerium Particles are typically 5 - 40 nanometers (nm) with specific su.. |
|||
Specific Surface Area | >= 30 m²/g | >= 30 m²/g | BET |
Oceanchem Group Magnesium Hydroxide Molecular Formula: Mg(OH)2Cas No.: 1309-42-8Use: Magnesium hydroxide is a non-halogen flame retardant recommended where use of halogenated products is limited or prohibited. In addition, it is an e.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Cobalt Iron Nanopowder General DescriptionCobalt Iron ( CoFe) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |