Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | BET |
Nabaltec ACTILOX® B20 AlO(OH) Boehmite Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature stabilitySynergistic effects with other flame retardantsHigh acid resistance.. |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | BET |
Nabaltec APYRAL® 22 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Specific Surface Area | 2.0 - 3.0 m²/g | 2.0 - 3.0 m²/g | BET |
Nabaltec NABALOX® NO 715-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 2.0 - 4.0 m²/g | 2.0 - 4.0 m²/g | |
NYC YT3X Y2O3 Powder |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | BET |
Nabaltec APYRAL® AOH 20 AlO(OH) Boehmite Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature applicationsLow sedimentation at good viscosity performance in resinsGood ch.. |
|||
Specific Surface Area | <= 2.0 m²/g | <= 2.0 m²/g | BET |
Magyar Aluminum ALO-G5-4 Alumina Ground Alumina |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | |
Momentive Performance Materials AC-6004 Boron Nitride (BN) Powder Grade AC-6004 is a high purity, fine (99%,-325 mesh) Boron Nitride (BN) powder with a hexagonal crystal structure and large graphite-like platelets. It exhibits the unique properties of boron nitri.. |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | |
Momentive Performance Materials HCJ-48 Boron Nitride (BN) Powder Grade HCJ-48 is a coarse (-20 mesh), hexagonal Boron Nitride (BN) powder with a mean particle size of 200-250µ. It exhibits the unique properties of BN in a form readily used in the production o.. |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | |
Momentive Performance Materials HCM Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powder grades HCR48, HCJ48, and HCM are large, high-density agglomerates, of ~10 µm crystals, with average particle sizes between 175-275 µm and tap den.. |
|||
Specific Surface Area | <= 2.0 m²/g | <= 2.0 m²/g | BET |
H.C. Starck Grade A Aluminum Nitride AIN High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon.. |
|||
Specific Surface Area | <= 2.0 m²/g | <= 2.0 m²/g | BET |
H.C. Starck Grade AT Aluminum Nitride AIN High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon.. |
|||
Specific Surface Area | 2.0 - 4.0 m²/g | 2.0 - 4.0 m²/g | BET |
H.C. Starck Grade B Aluminum Nitride AIN High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon.. |
|||
Specific Surface Area | 2.0 - 70 m²/g | 2.0 - 70 m²/g | |
Terio Corporation TZC-15~80 CeO2-ZrO2 Information provided by TERIO Corporation. |
|||
Specific Surface Area | 2.0 - 10 m²/g | 2.0 - 10 m²/g | |
American Elements Europium Nanoparticles General DescriptionEuropium (Eu) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Europium Particles are typically 10 - 45 nanometers (nm) with specif.. |
|||
Specific Surface Area | 2.0 - 10 m²/g | 2.0 - 10 m²/g | |
American Elements Carbon Nanoparticles General DescriptionCarbon (C) Nanoparticles, nanodots or nanopowder are black spherical high surface area graphitic carbon. Nanoscale Carbon Particles are typically 10 - 45 nanometers (nm) with spec.. |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | ATO 40-45-0 (BET) |
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6 Information provided by Arkema Group |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | |
Asahi Glass Fluon® L169J PTFE Lubricant Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As.. |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | |
BASF Theroplast® Red 454 Color Additive Chemical Structure: Monoazo RedApplication: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by BA.. |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | |
BASF Sicotan® Yellow K 1011 Color Additive Chemical Structure: Ni/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | |
BASF Sicotan® Yellow K 2112 Color Additive Chemical Structure: Cr/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | |
BASF Theroplast® Black X70 Color Additive Application: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, PA and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by BASF |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | |
BASF Theroplast® Blue 684 Color Additive Chemical Structure: AnthrachinonApplication: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by B.. |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | B.E.T. |
ATI Wah Chang Spectrographic Grade Zirconium Oxide, ZrO2 Spectrographic Grade. A fine, white powder.Information provided by ATI Wah Chang |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | BET; DIN 66132 |
3M Dyneon™ TF 9205 PTFE 3M™ Dyneon™ PTFE TF micropowders can be used as additives in many different applications and at concentrations typically from 5 to 20%. Homogeneous incorporation helps ensure optimum performance. .. |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | |
Momentive Performance Materials PolarTherm® PT370 Boron Nitride (BN) Powder Low Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic compon.. |
|||
Specific Surface Area | 2.0 m²/g | 2.0 m²/g | |
BASF Theroplast® Yellow 104 Color Additive Chemical Structure: Pyrazolone YellowApplication: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided.. |