Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 1.0 m²/g | 1.0 m²/g | BET |
Nyco NYGLOS® 12 Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Specific Surface Area | 1.0 - 2.0 m²/g | 1.0 - 2.0 m²/g | BET |
Nabaltec NABALOX® NO 115 TC Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 1.0 - 2.0 m²/g | 1.0 - 2.0 m²/g | BET |
Nabaltec NABALOX® NO 115-71 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 1.0 - 2.0 m²/g | 1.0 - 2.0 m²/g | BET |
Nabaltec NABALOX® NO 315 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 1.0 - 2.0 m²/g | 1.0 - 2.0 m²/g | BET |
Nabaltec NABALOX® NO 725-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | <= 1.0 m²/g | <= 1.0 m²/g | BET |
Magyar Aluminum ALO-DFM Alumina Alumina for Polishing |
|||
Specific Surface Area | <= 1.0 m²/g | <= 1.0 m²/g | BET |
Magyar Aluminum ALO-Ex34 Alumina Calcined Alumina |
|||
Specific Surface Area | <= 1.0 m²/g | <= 1.0 m²/g | BET |
Magyar Aluminum ALO-P54 Alumina Alumina for Polishing |
|||
Specific Surface Area | 1.0 m²/g | 1.0 m²/g | |
Momentive Performance Materials HCT-F Titanium Diboride (TiB2) Powder Grade HCT-F powders are designed for use on applications requiring reduced particle size without sacrificing high purity.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced.. |
|||
Specific Surface Area | <= 1.0 m²/g | <= 1.0 m²/g | BET |
H.C. Starck Grade A Molybdenum Disilicide MoSi2 Composite ceramicsHeating elementsConstituent of glow plugs for enginesRaw material for MoSi2 sputter target (PVD) |
|||
Specific Surface Area | 1.0 - 7.0 m²/g | 1.0 - 7.0 m²/g | BET |
H.C. Starck Grade AT Yttrium Oxide Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Specific Surface Area | >= 1.0 m²/g | >= 1.0 m²/g | BET |
H.C. Starck Grade C Molybdenum Disilicide MoSi2 Composite ceramicsHeating elementsConstituent of glow plugs for enginesRaw material for MoSi2 sputter target (PVD) |
|||
Specific Surface Area | 1.0 - 50 m²/g | 1.0 - 50 m²/g | |
Terio Corporation TZ-1~30 Zirconia Information provided by TERIO Corporation. |
|||
Specific Surface Area | 1.0 - 3.0 m²/g | 1.0 - 3.0 m²/g | |
American Elements Gold Nanoparticles General DescriptionGold (Au) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Gold Particles are typically 20 - 100 nanometers (nm) with specifi.. |
|||
Specific Surface Area | 1.0 - 5.0 m²/g | 1.0 - 5.0 m²/g | |
American Elements Iridium Nanoparticles General DescriptionIridium (Ir) Nanoparticles, nanodots or nanopowder are black spherical high surface area metal particles. Nanoscale Iridium Particles are typically 20 - 100 nanometers (nm) with s.. |
|||
Specific Surface Area | 1.0 - 5.0 m²/g | 1.0 - 5.0 m²/g | |
American Elements Molybdenum Nanoparticles General DescriptionMolybdenum (Mo) Nanoparticles, nanodots or nanopowder are black high surface area particles. Nanoscale Molybdenum Particles are typically 50 - 100 nanometers (nm) with specific su.. |
|||
Specific Surface Area | 1.0 - 3.0 m²/g | 1.0 - 3.0 m²/g | |
American Elements Palladium Nanoparticles General DescriptionPalladium (Pd) Nanoparticles, nanodots or nanopowder are black spherical high surface area metal particles. Nanoscale Palladium Particles are typically 20 - 100 nanometers (nm) wi.. |
|||
Specific Surface Area | 1.0 - 3.0 m²/g | 1.0 - 3.0 m²/g | |
American Elements Platinum Nanoparticles General DescriptionPlatinum (Pt) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Platinum Particles are typically 20 - 100 nanometers (nm) with.. |
|||
Specific Surface Area | 1.0 - 3.0 m²/g | 1.0 - 3.0 m²/g | |
American Elements Rhenium Nanoparticles General DescriptionRhenium (Re) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Rhenium Particles are typically 20 - 100 nanometers (nm) with s.. |
|||
Specific Surface Area | 1.0 - 3.0 m²/g | 1.0 - 3.0 m²/g | |
American Elements Ruthenium Nanoparticles General DescriptionRuthenium (Ru) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Ruthenium Particles are typically 20 - 100 nanometers (nm) wi.. |
|||
Specific Surface Area | 1.0 m²/g | 1.0 m²/g | |
American Elements Silver Nanoparticles General DescriptionSilver (Ag) Nanoparticles, nanodots or nanopowder are spherical or flake high surface area metal particles. Nanoscale Silver Particles are typically 1 - 40 nanometers (nm) with sp.. |
|||
Specific Surface Area | 1.0 m²/g | 1.0 m²/g | |
American Elements Silver Nanoparticles General DescriptionSilver (Ag) Nanoparticles, nanodots or nanopowder are spherical or flake high surface area metal particles. Nanoscale Silver Particles are typically 1 - 40 nanometers (nm) with sp.. |
|||
Specific Surface Area | 1.0 - 5.0 m²/g | 1.0 - 5.0 m²/g | |
American Elements Titanium Nanoparticles General DescriptionTitanium (Ti) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Titanium Particles are typically 10 - 80 nanometers (nm) .. |
|||
Specific Surface Area | 1.0 m²/g | 1.0 m²/g | Cloth |
Cytec Thornel® Graphite Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Specific Surface Area | 1.0 m²/g | 1.0 m²/g | |
Cytec Thornel® VCB-20 Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Used as a reinforcement in structural, ablative, and abrasion-resistant composites.2000 filaments/strand, 99+% carbon assayThornel®.. |
|||
Specific Surface Area | 1.0 m²/g | 1.0 m²/g | Cloth |
Cytec Thornel® VCK Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Specific Surface Area | 1.0 m²/g | 1.0 m²/g | Cloth |
Cytec Thornel® VCL Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Specific Surface Area | 1.0 m²/g | 1.0 m²/g | ATO 40-45-0 (BET) |
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved Information provided by Arkema Group |
|||
Specific Surface Area | 1.0 m²/g | 1.0 m²/g | ATO 40-45-0 (BET) |
Arkema Group ORGASOL® 2002 ES 5 Nat 3 Polyamide 12 Information provided by Arkema Group |
|||
Specific Surface Area | 1.0 m²/g | 1.0 m²/g | |
BASF Theroplast® F Yellow 084 Color Additive Chemical Structure: PeryleneApplication: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by BASF |