Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 5.0 - 8.0 m²/g | 5.0 - 8.0 m²/g | BET |
Magyar Aluminum ALOLT 90DLS Aluminum Hydroxide Fine Precipitated Type |
|||
Specific Surface Area | 5.0 - 8.0 m²/g | 5.0 - 8.0 m²/g | BET |
Magyar Aluminum ALOLT 90F Aluminum Hydroxide Fine Precipitated Type |
|||
Specific Surface Area | 3.0 - 8.0 m²/g | 3.0 - 8.0 m²/g | BET |
Magyar Aluminum ALO-P95-01 Alumina Alumina for Polishing |
|||
Specific Surface Area | 3.0 - 8.0 m²/g | 3.0 - 8.0 m²/g | BET |
Magyar Aluminum ALO-P95-06 Alumina Alumina for Polishing |
|||
Specific Surface Area | 3.0 - 8.0 m²/g | 3.0 - 8.0 m²/g | BET |
Magyar Aluminum ALO-P95-08 Alumina Alumina for Polishing |
|||
Specific Surface Area | 4.0 - 8.0 m²/g | 4.0 - 8.0 m²/g | BET |
H.C. Starck Grade C Aluminum Nitride AIN High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon.. |
|||
Specific Surface Area | 6.0 - 8.0 m²/g | 6.0 - 8.0 m²/g | Low range |
Vesta Ceramics SicoNide® P Silicon Nitride Powder General Description:SicoNide® is a silicon nitride powder with a broad particle size distribution allowing better, tighter packing when pressed. Our computer-controlled production processes guaran.. |
|||
Specific Surface Area | 6.0 - 8.0 m²/g | 6.0 - 8.0 m²/g | Low range |
Vesta Ceramics SicoNide® S S Silicon Nitride Powder General Description:SicoNide® is a silicon nitride powder with a broad particle size distribution allowing better, tighter packing when pressed. Our computer-controlled production processes guaran.. |
|||
Specific Surface Area | 6.0 - 8.0 m²/g | 6.0 - 8.0 m²/g | |
Dandong Taico Minerals TAICOCITE® TC12 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Specific Surface Area | 6.0 - 8.0 m²/g | 6.0 - 8.0 m²/g | |
Dandong Taico Minerals TAICOCITE® TC35 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Specific Surface Area | 6.0 - 8.0 m²/g | 6.0 - 8.0 m²/g | |
Dandong Taico Minerals TAICOCITE® TC50 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Specific Surface Area | 6.0 - 8.0 m²/g | 6.0 - 8.0 m²/g | |
Dandong Taico Minerals TAICOCITE® TC8 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Specific Surface Area | 6.0 - 8.0 m²/g | 6.0 - 8.0 m²/g | |
Dandong Taico Minerals TAICOCITE® TC3 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Specific Surface Area | 6.0 - 8.0 m²/g | 6.0 - 8.0 m²/g | |
Dandong Taico Minerals TAICOCITE® TC80 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Specific Surface Area | 4.0 - 8.0 m²/g | 4.0 - 8.0 m²/g | B.E.T. |
ATI Wah Chang Jet Milled Zirconium Oxide, ZrO2 Jet Milled. A fine, white powder.Information provided by ATI Wah ChangTypical Analysis: On Zr oxide basis |
|||
Specific Surface Area | 3.0 - 8.0 m²/g | 3.0 - 8.0 m²/g | |
Momentive Performance Materials PolarTherm® PT140 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Specific Surface Area | 3.0 - 8.0 m²/g | 3.0 - 8.0 m²/g | |
Momentive Performance Materials PolarTherm® PT350 Boron Nitride (BN) Powder Low Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic compon.. |