Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 50 - 70 m²/g | 50 - 70 m²/g | BET |
Nabaltec NABALOX® NO 201 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 60 - 70 m²/g | 60 - 70 m²/g | |
NanoAmor 95%, OD/L: 40-60 nm/1-2 um Multi-Walled Carbon Nanotubes |
|||
Specific Surface Area | 60 - 70 m²/g | 60 - 70 m²/g | |
NanoAmor 99%, OD/L: 40-60 nm/1-2 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Specific Surface Area | 2.0 - 70 m²/g | 2.0 - 70 m²/g | |
Terio Corporation TZC-15~80 CeO2-ZrO2 Information provided by TERIO Corporation. |
|||
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Aluminum Nanoparticles General DescriptionAluminum (Al) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Aluminum Particles are typically 10-30 nanometers (nm) with sp.. |
|||
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Beryllium Nanoparticles General DescriptionBeryllium (Be) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Beryllium Particles are typically 20-60 nanometers (nm) with specif.. |
|||
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Magnesium Nanoparticles General DescriptionMagnesium (Mg) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Magnesium Particles are typically 20-60 nanometers (nm) with specif.. |
|||
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Silicon Nanoparticles General DescriptionSilicon (Si) Nanoparticles, nanodots or Nanopowder are spherical high surface area metal particles. Nanoscale Silicon Particles are typically 5-25 nanometers (nm) with specific su.. |
|||
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Cobalt Nanoparticles General DescriptionCobalt (Co) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Cobalt Particles are typically 20-60 nanometers (nm) with specific sur.. |
|||
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Copper Nanoparticles General DescriptionCopper (Cu) Nanoparticles, nanodots or Nanopowder are black brown spherical high surface area metal particles. Nanoscale Copper Particles are typically 10-30 nanometers (nm) with .. |