Physical Properties Metric English Comments
Specific Surface Area 250 - 300 m²/g
250 - 300 m²/g
BET
Nanocyl NANOCYL™ NC7000 Thin Multi-Wall Carbon Nanotubes
NANOCYL™ NC7000 Series, thin multi-wall carbon nanotubes, are produced via the catalytic carbon vapor deposition (CCVD) process.These carbon nanotubes are unique and prized world-wide because their..
Specific Surface Area 40 - 300 m²/g
40 - 300 m²/g
NanoAmor 95% 10-20 nm Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Specific Surface Area 10 - 300 m²/g
10 - 300 m²/g
Terio Corporation TZOH-40 Zirconium Hydroxide
Information provided by TERIO Corporation.
Specific Surface Area 10 - 300 m²/g
10 - 300 m²/g
Terio Corporation TZOH-50 Zirconium Hydroxide
Information provided by TERIO Corporation.
Specific Surface Area 10 - 300 m²/g
10 - 300 m²/g
Terio Corporation TZOH-60 Zirconium Hydroxide
Information provided by TERIO Corporation.