Polymer Property : Specific Surface Area = 3.3 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 3.3 m²/g
3.3 m²/g
Omya OMYACARB® 520 - FL Calcium Carbonate
A high purity, fine, wet ground natural calcium carbonate surface-treated and activated for low humidity content.Applications: Adhesive applications where low moisture content and pick up is require..