Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 200 m²/g | 200 m²/g | |
NanoAmor 90%, OD/ID: 10-30/3-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Specific Surface Area | 200 m²/g | 200 m²/g | |
NanoAmor 95%, OD/ID/L: 10-20/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Specific Surface Area | 200 - 350 m²/g | 200 - 350 m²/g | |
NanoAmor 95%, OD/ID: 10-20/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Specific Surface Area | 200 m²/g | 200 m²/g | |
NanoAmor 95%, OD: 10-20 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Specific Surface Area | 200 m²/g | 200 m²/g | |
NanoAmor 95%, OD: 10-20 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |