Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 180 m²/g | 180 m²/g | |
Zircar Ceramics AL-R/H Alumina Rigidizer/Hardener Type AL-R/H Alumina Rigidizer/Hardener is a single part water based colloidal suspension of alumina hydrate. Mainly used for rigidizing and hardening the surfaces of ZIRCAR® fibrous ceramic product.. |