Polymer Property : Specific Surface Area = 14 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 14 m²/g
14 m²/g
Momentive Performance Materials NX10 Boron Nitride (BN) Powder
Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades a..
Specific Surface Area 14 m²/g
14 m²/g
Momentive Performance Materials PolarTherm® PT131 Boron Nitride (BN) Powder
Boron Nitride powders are produced by GE Advanced Ceramics in more than 50 individual (standard and custom) grades to meet a wide variety of application needs.For use in: Electrically insulating/the..
Specific Surface Area 14 - 16 m²/g
14 - 16 m²/g
BET
H.C. Starck Grade UF 15 Silicon Carbide, SiC
Alpha SiC for sintering.Sliding bearingsSeal ringsWear partsKiln furniture, crucibles, heating elements, burner nozzles, heat exchangersSemiconductor handling partsComponents for wafer processing (s..
Specific Surface Area 14 - 15 m²/g
14 - 15 m²/g
External
St. Cloud Natural Zeolite (Clinoptilolite)
Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter..
Specific Surface Area 14 m²/g
14 m²/g
3pt. B.E.T.
Zircar Refractory Composites RS-99R Refractory Sheet
Type RS-99R boards are prefired and are unaffected by moisture. They stay rigid even if saturated with water.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
Specific Surface Area >= 14 m²/g
>= 14 m²/g
Internal Method
Solvay Specialty Polymers Algoflon® L101-1 Polytetrafluoroethylene (PTFE)  (Unverified Data**)
Algoflon® L101-1 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It exhibits excellent chemical and heat resistance, low surface energy and low coefficient ..