Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 12.5 m²/g | 12.5 m²/g | |
Omya COVERCARB® 85 Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating that is designed to provide maximum opacity and maximum gloss. It is an excellent choice to reduce the demand for expensive pigments.. |
|||
Specific Surface Area | 12.5 m²/g | 12.5 m²/g | |
Omya HYDROCARB® 90 Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Specific Surface Area | 12.5 m²/g | 12.5 m²/g | |
Omya HYDROCARB® 90 HS Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Specific Surface Area | 12.5 m²/g | 12.5 m²/g | |
Omya HYDROCARB® 95 HS Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Specific Surface Area | 12.5 m²/g | 12.5 m²/g | |
Imerys Kingsleyâ„¢ Kaolin Kingsley is a coarse-grained, white firing kaolin used in the dinnerware, tile, artware and electrical porcelain industries.Information provided by Imerys |
|||
Specific Surface Area | 12.5 m²/g | 12.5 m²/g | |
BASF Paliotan® Yellow L 1145 Color Additive Description: Pigment combination based on Bismuth VanadateSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, and Airdrying systems.Information provided by BASF |