Physical Properties Metric English Comments
Specific Surface Area 12 m²/g
12 m²/g
Omya OMYACARB® UF - FL Calcium Carbonate
A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water..
Specific Surface Area 12 m²/g
12 m²/g
Omya OMYAFLOW® UF - SY Calcium Carbonate
A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Decorative paints.Information supplied by Omya North America.
Specific Surface Area 12 - 20 m²/g
12 - 20 m²/g
NYC YT3CP Y2O3 Powder
Specific Surface Area 12 - 30 m²/g
12 - 30 m²/g
BET
Magyar Aluminum ALO-Ex32 Alumina
Calcined Alumina
Specific Surface Area 12 - 30 m²/g
12 - 30 m²/g
BET
Magyar Aluminum ALO-G2-2 Alumina
Ground Alumina
Specific Surface Area 12 - 15 m²/g
12 - 15 m²/g
Imerys Alumexâ„¢ Kaolin
Alumex is a Hydrated Aluminum Silicate used as a low surface area “soft” filler for Elastomeric systems.Information provided by Imerys
Specific Surface Area 12 - 15 m²/g
12 - 15 m²/g
Imerys Hydrated Aluminum Silicate KT 90A-1 Kaolin
KT 90A-1 is a Hydraetd Aluminum Silicate. It is a high surface area, fine particle size clay that is well suited for use as an econoMical filler.Information provided by Imerys
Specific Surface Area 12 - 15 m²/g
12 - 15 m²/g
Imerys Kaolexâ„¢ FG Kaolin
Kaolex FG is a air floated Hydrated Aluminum Silicate. Its low surface area makes it a good choice for fiberglass manufacturing.Information provided by Imerys
Specific Surface Area 12 - 15 m²/g
12 - 15 m²/g
Imerys Kaolexâ„¢ SC Kaolin
Kaolex SC is an air floated Hydrated Aluminum Silicate. It is a low surface area, low viscosity, medium casting filler/extender for ceramic applications.Information provided by Imerys
Specific Surface Area 12 m²/g
12 m²/g
Imerys KT Castâ„¢ Kaolin
KT Cast is a coarse-grained, white firing kaolin that is used primarily in casting bodies based on its fast casting and exceptional deflocculation characteristics.Information provided by Imerys
Specific Surface Area 12 - 15 m²/g
12 - 15 m²/g
BET
H.C. Starck Grade M11 h.p. Silicon Nitride, Si3N4
Higher purity, >99.995%Ceramic cutting toolsHeavy duty components in automotive enginesHigh performance parts for mechanical engineeringBearing components, like high precision ballsSiAlONsMetallurgy..
Specific Surface Area 12 - 15 m²/g
12 - 15 m²/g
BET
H.C. Starck Grade M11 I.o. Silicon Nitride, Si3N4
Alpha-phase > 90%, low oxygen content
Specific Surface Area 12 - 15 m²/g
12 - 15 m²/g
BET
H.C. Starck Grade M11 Silicon Nitride, Si3N4
Alpha-phase > 90%, very narrow particle size distribution.Ceramic cutting toolsHeavy duty components in automotive enginesHigh performance parts for mechanical engineeringBearing components, like hi..
Specific Surface Area 12 m²/g
12 m²/g
American Elements Niobium Nanoparticles
General DescriptionNiobium (Nb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Niobium Particles are typically 10-20 nanometers (nm) with..
Specific Surface Area 12 m²/g
12 m²/g
American Elements Tantalum Nanoparticles
General DescriptionTantalum (Ta) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tantalum Particles are typically 10-20 nanometers (nm) wi..
Specific Surface Area 12 m²/g
12 m²/g
American Elements Tin Nanoparticles
General DescriptionTin (Sn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tin Particles are typically 10-20 nanometers (nm) with specifi..