Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 35 - 55 µm | 35 - 55 µm | |
Lucite International Colacryl ® TS1742 Acrylic Dental Resin Lucite® Colacryl® TS1742 is a plasticiser free, ethyl methacrylate based resin aimed at the formulation of heat-cured, soft materials, such as ear moulds, where it is well suited to use with C.. |
|||
Particle Size | 45 - 55 µm | 45 - 55 µm | |
Lucite International Colacryl ® TS1785 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I.. |
|||
Particle Size | 40 - 55 µm | 40 - 55 µm | d90, Guaranteed |
TIMCAL TIMREX® LSG 44 Natural Graphite Flakes TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 35 - 55 µm | 35 - 55 µm | D(0.5) |
Akzo Nobel Expancel® 091 WE 40 d24 Wet expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 35 - 55 µm | 35 - 55 µm | D(0.5) |
Akzo Nobel Expancel® 461 DE 40 d25 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 35 - 55 µm | 35 - 55 µm | D(0.5) |
Akzo Nobel Expancel® 461 DET 40 d25 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 35 - 55 µm | 35 - 55 µm | D(0.5) |
Akzo Nobel Expancel® 091 DE 40 d30 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |